Looking for an internshipMay 24 to August 31, 2027

Back to projects

Floors

The values pass: why ask for recompaction?

100 MPa

EV2 moduli above 100 MPa against 50 required, and a recommendation to recompact with moistening, sent with the test report.

The constraints

A platform to check before slab pouring, at 3 measurement points, with a 50 MPa requirement on the EV2 modulus.

My role

Work-study test technician at EuroContrôle Qualité, from September 2024 to August 2025, handling about 50 assignments independently.

What I did

On site, static plate load tests (LCPC CT2 procedure, 600 mm plate, Benkelman beam, EV1 and EV2 moduli) and light dynamic plate tests.

In the lab, standard tests: methylene blue value, sieve analysis, immediate bearing index.

From these tests, soil classification to the French GTR 92 guide, to decide on reuse, treatment or rejection.

How I checked it

The EV2 moduli exceed the requirement, but the EV2/EV1 ratio exceeds 2.2. The two values have to be read together.

Still to write

[to be completed with Léo: a photo or a figure, chosen together]

[to be completed with Léo: the reasoning in plain words]

[to be completed with Léo: what came of the recommendation, if known]

Arrow keys scroll, Enter keeps the rendering, Escape goes back to the previous one.